Status de disponibilidade: | |
---|---|
Quantidade: | |
Material: liga 825/n08825, tp316/l, tp304/l, s32205, s32750, liga 400/n04400, liga 625/n06625
Pacote: carretel de madeira ou ferro
![]() | ![]() |
Nota | C max | Si Max | Mn Max | P max | S max | Cr | Ni | MO | Ti | N máx | Cu max | Nb | Al max | Co max | Zr | Fe Max | Tu | VA |
Alloy 600/N06600 | 0 | 1 | 1 | - | 0 | 14-17 | ≥72 | - | - | - | 1 | - | - | - | - | 6-10 | - | - |
Alloy 601/N06601 | 0 | 1 | 2 | - | 0 | 21.0-25.0 | 58-63 | - | - | - | 1 | - | 1.0-1.7 | - | - | - | - | - |
Alloy 625/N06625 | 0 | 1 | 1 | 0 | 0 | 20-23 | ≥58 | 8-10 | <0,4 | - | - | 3.15-4.15 | ≤0,4 | - | - | 5.00 restante | - | - |
Alloy 718/N07718 | 0 | 0 | 0 | 0 | 0 | 17.0-21.0 | 50.0-55.0 | 2.8-3.3 | 0,65-1.15 | 0 | 0 | 4.75-5.5 | 0,2-0.8 | 1 | - | - | - | - |
Alloy 800/N08800 | 0 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0,15-0,60 | - | 1 | - | 0,15-0,60 | - | - | ≥39,5 | - | - |
Liga 800h/n08810 | 0,05-0.10 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0,15-0,60 | - | 1 | - | 0,15-0,60 | - | - | ≥39,5 | - | - |
Alloy 825/N08825 | 0 | 1 | 1 | - | 0 | 19.5-23.5 | 38-46 | 2.5-3.5 | 0,6-1.2 | - | 1.5-3 | - | 0 | - | - | ≥22 | - | - |
Nota | Propriedade física | |||
Ys | Ts | El. | Hb | |
Alloy 600/N06600 | 205-345 | 550-690 | 35-55 | ≤185 |
Alloy 601/N06601 | 240-300 | 600-650 | 30-35 | ≤220 |
Alloy 625/N06625 | ≥345 | ≥760 | ≥30 | ≤220 |
Alloy 718/N07718 | ≥550 | ≥965 | ≥30 | ≤363 |
Alloy 800/N08800 | ≥210 | ≥500 | ≥35 | - |
Liga 800h/n08810 | ≥180 | ≥450 | ≥35 | - |
Alloy 825/N08825 | ≥220 | ≥550 | ≥30 | ≤200 |
1. Transferência de gases e líquidos usados para aquecimento, resfriamento e uma variedade de outros propósitos.
2. Equipamento médico.
3. Energia solar.
4. Encanamento.
5. Moletolos de gás.
6. Condensador da superfície do vapor.
Material: liga 825/n08825, tp316/l, tp304/l, s32205, s32750, liga 400/n04400, liga 625/n06625
Pacote: carretel de madeira ou ferro
![]() | ![]() |
Nota | C max | Si Max | Mn Max | P max | S max | Cr | Ni | MO | Ti | N máx | Cu max | Nb | Al max | Co max | Zr | Fe Max | Tu | VA |
Alloy 600/N06600 | 0 | 1 | 1 | - | 0 | 14-17 | ≥72 | - | - | - | 1 | - | - | - | - | 6-10 | - | - |
Alloy 601/N06601 | 0 | 1 | 2 | - | 0 | 21.0-25.0 | 58-63 | - | - | - | 1 | - | 1.0-1.7 | - | - | - | - | - |
Alloy 625/N06625 | 0 | 1 | 1 | 0 | 0 | 20-23 | ≥58 | 8-10 | <0,4 | - | - | 3.15-4.15 | ≤0,4 | - | - | 5.00 restante | - | - |
Alloy 718/N07718 | 0 | 0 | 0 | 0 | 0 | 17.0-21.0 | 50.0-55.0 | 2.8-3.3 | 0,65-1.15 | 0 | 0 | 4.75-5.5 | 0,2-0.8 | 1 | - | - | - | - |
Alloy 800/N08800 | 0 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0,15-0,60 | - | 1 | - | 0,15-0,60 | - | - | ≥39,5 | - | - |
Liga 800h/n08810 | 0,05-0.10 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0,15-0,60 | - | 1 | - | 0,15-0,60 | - | - | ≥39,5 | - | - |
Alloy 825/N08825 | 0 | 1 | 1 | - | 0 | 19.5-23.5 | 38-46 | 2.5-3.5 | 0,6-1.2 | - | 1.5-3 | - | 0 | - | - | ≥22 | - | - |
Nota | Propriedade física | |||
Ys | Ts | El. | Hb | |
Alloy 600/N06600 | 205-345 | 550-690 | 35-55 | ≤185 |
Alloy 601/N06601 | 240-300 | 600-650 | 30-35 | ≤220 |
Alloy 625/N06625 | ≥345 | ≥760 | ≥30 | ≤220 |
Alloy 718/N07718 | ≥550 | ≥965 | ≥30 | ≤363 |
Alloy 800/N08800 | ≥210 | ≥500 | ≥35 | - |
Liga 800h/n08810 | ≥180 | ≥450 | ≥35 | - |
Alloy 825/N08825 | ≥220 | ≥550 | ≥30 | ≤200 |
1. Transferência de gases e líquidos usados para aquecimento, resfriamento e uma variedade de outros propósitos.
2. Equipamento médico.
3. Energia solar.
4. Encanamento.
5. Moletolos de gás.
6. Condensador da superfície do vapor.